Batch flotation tests were conducted on a haematite-bearing Sishen iron ore slimes sample from South Africa using reverse cationic flotation. The effect of grinding on flotation performance, the flotation response of various key impurities in the sample, and the feasibility of increasing metal recovery by refloating tailings in a scavenger flotation step were investigated. The test results indicate that reverse cationic flotation is effective in rejecting impurities from the iron ore sample tested. From a head grade assaying 6.4 per cent SiO2, 2.14 per cent Al2O3, 0.402 per cent K2O, 0.082 per cent P and 0.194 per cent TiO2, the levels of impurities were reduced to 1.83 per cent SiO2, 0.88 per cent Al2O3, 0.095 per cent K2O, 0.066 per cent P and 0.174 per cent TiO2 in the final concentrate at a Fe recovery of 74 per cent. The flotation response of SiO2, Al2O3 and K2O were found to be better than that of P and TiO2. The testwork demonstrated that grinding to 80 per cent passing about 49 microns is essential for upgrading the Sishen iron ore to produce >67 per cent Fe concentrate grade. This grind size corresponds to about 80 per cent liberation of haematite from the gangue minerals. Fe recoveries up to 76 per cent were obtained by refloating the rougher tailings in a scavenger stage, with little effect on the final concentrate grade. Size-by-size Fe recovery data obtained indicated that particles below ten microns were mostly lost in the desliming stage conducted prior to flotation whilst some reported to the froth by entrainment. Some of the coarser haematite-gangue composite particles reported to the froth product by genuine flotation.
Return to parent product
  • Upgrading Sishen Iron Ore Slimes by Reverse Cationic Flotation
    PDF
    This product is exclusive to Digital library subscription
  • Upgrading Sishen Iron Ore Slimes by Reverse Cationic Flotation
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 2008
  • PDF Size: 0.111 Mb.
  • Unique ID: P200907046

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.