Removal of Phosphorous from Australian Iron Ores

Phosphorous is typically present in iron ore either in the mineral apatite, Ca5(PO4)3OH, or associated with the goethitic fraction of the ore. In this paper, we present results that show that phosphorous associated with the goethitic fraction can be removed with a heating pretreatment around 300C for 1 h, followed by a caustic leach with 1 - 5 M NaOH, or a leach with sulfuric acid at pH 0.5. The heating pretreatment is considered to dehydroxylate the goethite to form a haematite intermediate phase, protohaematite', that reacts during the leach making the phosphorous accessible to the leachant. In the acid leach, ten to 15 per cent of the sample was dissolved to obtain a leach product with 0.08 per cent P. In the caustic leach, as no weight loss occurs, it is proposed that iron species associated with the protohaematite have either not dissolved or have reprecipitated at the high pH values of the leach.For an ore containing apatite as the source of phosphorous, a leach with sulfuric acid dissolved the apatite, lowering the phosphorous levels in the sample. The sample treated contained carbonate minerals (including siderite) that also reacted with the acid, and in practice a balance between the dissolution of the apatite and the carbonate minerals may be needed to minimise acid consumption.
Return to parent product
  • Removal of Phosphorous from Australian Iron Ores
    PDF
    This product is exclusive to Digital library subscription
  • Removal of Phosphorous from Australian Iron Ores
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 2011
  • PDF Size: 0.187 Mb.
  • Unique ID: P201106053

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.