Effects of Alternate Methods of Conditioning on the Reflotation of Copper Concentrates at WMC (Olympic Dam Operations)

The effect of various methods of conditioning on subsequent flotation performance was reviewed, where complex interactions involving attrition, aggregation, dispersion and surface cleaning were discussed. The present study focussed on the influences of standard laboratory cell conditioning, ultrasonic dispersion and high intensity conditioning on copper mineral flotation characteristics. The effect of substituting demineralised water for the WMC plant water was also examined. It was found that higher copper concentrate grades were often obtained using demineralised water, however the use of high intensity conditioning in mill water gave the highest copper recovery and highest flotation rate constant. This process should be considered if copper grade and recovery in this section of the plant drops, especially if the drop is due to surface oxidation of the copper minerals. Other methods of conditioning (cell and ultrasonic techniques) improved the rate of copper flotation above that obtained in the virtual absence of conditioning, showing the importance of conditioning on subsequent flotation operations.
Return to parent product
  • Effects of Alternate Methods of Conditioning on the Reflotation of Copper Concentrates at WMC (Olympic Dam Operations)
    PDF
    This product is exclusive to Digital library subscription
  • Effects of Alternate Methods of Conditioning on the Reflotation of Copper Concentrates at WMC (Olympic Dam Operations)
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 1999
  • PDF Size: 0.549 Mb.
  • Unique ID: P200005047

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.