Sulphuric Acid Leaching of Manganese Nodules in the Presence of Charcoal

Leaching studies were carried out on Indian Ocean manganese nodules using sulphuric acid as the lixiviant. By leaching the nodules with 8 per cent sulphuric acid for 12h at 100C, copper and nickel could be completely extracted along with 50 per cent cobalt and 6.2 per cent manganese.94.2 per cent of the iron was also dissolved. To increase manganese and cobalt extraction, charcoal was used as a reductant. The role of charcoal was to reduce the manganese dioxide and render it soluble as manganese sulphate as well as to facilitate solution of the cobalt minerals associated with the manganese dioxide. Various leaching parameters were studied including acid concentration, amount of reductant, leach time, pulp density and leach temperature. It was found that by leaching the nodules with 10 per cent sulphuric acid at 100C for 4h using 5 wt/wt per cent charcoal (0.05g of charcoal per g of nodule) almost complete extraction of copper, nickel, cobalt and manganese could be achieved. However, under these conditions all the iron present in the nodules was also leached.
Return to parent product
  • Sulphuric Acid Leaching of Manganese Nodules in the Presence of Charcoal
    PDF
    This product is exclusive to Digital library subscription
  • Sulphuric Acid Leaching of Manganese Nodules in the Presence of Charcoal
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 1989
  • PDF Size: 0.723 Mb.
  • Unique ID: P_PROC1989_1737

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.